J. Appl. Mech. September 2006, 73(5): 860–870.
Published Online: October 8, 2004
... for by increases in the intrinsic toughness as the traction-separation law varied with mode-mix. As a result, viscoplastic dissipation outside the cohesive zone was minimal. Atomic force fractography and X-ray photoelectron spectroscopy indicated that the crack growth mechanisms and the loci of fracture...