Optimization of weight, cost, and performance of deepwater offshore structures demands the increased utilization of high strength, light weight, and corrosion resistant materials such as titanium alloys. Titanium alloy Ti-6Al-4V has been considered for several critical components such as risers and taper joints. Because of the novelty of use of titanium alloys in the offshore industry, there is currently no standard governing design of titanium components for offshore structures. Since these structural components are subjected to a complex spectrum of environmental loading, assessment of defect tolerance using fatigue crack growth analysis is generally considered an important design parameter. In this paper, more than 60 crack growth data sets from 20 independent laboratories were collected and analyzed to develop crack growth rate equations for use in defect assessment. These data include the results of fatigue testing of both base material and welded joints in air and seawater with and without cathodic protection and at different R-ratios and test frequencies. The results suggest that for crack growth rates above 107in./cycle, crack growth of Ti-6Al-4V appears to be independent of testing condition and materials processing. At the low crack growth rate (below 107in./cycle), the review revealed that data are very limited. These limited data, however, suggest that the crack growth threshold is dependent on the R-ratio and slightly dependent on material processing. Comparison between crack growth rates of steel and titanium alloy (Ti-6Al-4V) showed that the two materials have very similar behavior.

1.
Herman, J. R., 1991, “Titanium Tapered Joint Applications,” Proc., ASME 10th Int. Conference of OMAE, Vol. III, Part A, eds., M. M. Salama et al., pp. 299–304.
2.
Salama
,
M. M.
,
Murali
,
J.
, and
Joosten
,
M. W.
,
2000
, “
Titanium Drilling Risers - Application and Qualification
,”
ASME J. Offshore Mech. Arct. Eng.
,
122
, pp.
47
51
.
3.
Salama, M. M., 1990, “Low-Temperature Properties of Structural Steel,” Metals Handbook, Vol. 1, 10th Ed., ASM International, pp. 662–672.
4.
BSI PD 6493, 1991, “Guidance on Methods for Assessing the Acceptability of Flaws in Fusion Welded Structures,” pp. 48–49.
5.
Booth
,
G. S.
, and
Dobbs
,
S.
,
1986
, “
Corrosion Fatigue Crack Growth in BS 4360 Grade 50D Steel
,”
Welding Institute Research Bulletin
,
27
(
9
), pp.
293
297
.
6.
Azkarate, I., Recio, A., and Del Barrio, A., 1992, “Environment Sensitive Stress Cracking of Titanium Alloys,” 7th World Conference on Titanium - San Diego, (preprint from the authors, INASMET, San Sebastian, Spain).
7.
Beach, J. E., and Marchica, N. V., 1978, “A Fatigue Comparison of High Strength Steel, Stainless Steel, and Titanium in Simulated Ocean Environment,” Proc., 10th Annual OTC, OTC 3253, Vol. 3, pp. 1737–1745.
8.
Belza, E., Eizaguirre, I., Santamaria, F., Irisarri, A. M., Plaza, L. M., and Rekondo, 1991, “Fatigue Crack Growth Behavior of Titanium Grade 2 Weldments,” Welding 91, Paris, France (preprint from the authors, INASMET, San Sebastian, Spain).
9.
Elber, W., 1975, “Crack-Closure and Crack-Growth Measurements in Surface-Flawed Titanium Alloy Ti-6Al-4V,” NASA Report No. NASA TN D-8010, Washington, DC.
1.
Gangloff, R. P., 1989, “Corrosion Fatigue Crack Propagation in Metals,” Environment-Induced Cracking of Metals Proceedings, NACE, pp. 55–109;
2.
(Titanium data after:
Dawson
,
D. B.
, and
Pelloux
,
R. M.
,
1974
,
Metall. Trans.
,
5
, pp.
72
731
.
1.
Halliday
,
M. D.
,
Blom
,
A. E.
, and
Beevers
,
C. J.
,
1989
, “
Potential Difference Applied to the Measurement of Small Fatigue Crack Growth at Notches in Ti-6Al-4V
,”
Scand. J. Metall.
,
18
, pp.
191
196
.
2.
Harrigan, M. J., 1972, “Fracture Mechanics Data for Air Force Handbook Usage,” Report TFD-72-501-1, North America Rockwell, Los Angeles, CA, Damage Tolerant Design Handbook, Metals and Ceramics information Center - Battelle, 1973, Figures NTA4-A23.
1.
Jaske, C. E., Payer, J. H., and Balint, V. S., 1981, “Corrosion Fatigue of Metals in Marine Environment,” Metals and Ceramics Information Center - Report MCIC-81-42, Battelle -Columbus Laboratories, Chap 8, pp. 201–243;
2.
reference paper by A. W. Rider, W. E. Krupp, D. E. Pettit, and D. W. Hoeppner on Corrosion Fatigue Properties of Recrystallization Annealed Ti-6Al-4V, ASTM-STP-642, 1977, pp. 202–222.
1.
Nippon Steel, 1992, “Test Procedure—Environment Assisted Fracture Properties of Ti-6Al-4V Plate and its Weld,” Nippon Steel Corporation Report, March 4, Steel Research Lab., Technical Development Bureau.
2.
Rockwell International, 1973, “Fracture Toughness Data Collection, Rockwell International Corporation, from B-1 Program,” Rockwell International, Los Angeles, CA, Damage Tolerant Design Handbook, Metals and Ceramics Information Center-Battelle, 1973, Figures NTA4-A23.
3.
Shida, Y. (Sumitomo Metal), 1991, private correspondence with Liv Lunde dated May 16, 1991 (reported in: Evaluation of Titanium Drilling Riser for Heidrun TLP by Liv Lunde and Mitchell Dziekonski).
4.
Soboyejo, W. O., 1991, “The Effect of Constraint on the Fatigue and Fracture Behavior of Recrystallization Annealed Ti-6Al-4V,” ASTM Symposium on Constraint in Fracture, May 8–9 1991, Indianapolis, IN.
5.
Sumitomo, Metal Industries, 1989, “Corrosion fatigue of Ti-6Al-4V,” Report by Sumitomo Metal Industries, Ltd., Japan (author unknown).
6.
Sumitomo, Metal Industries, 1991, “Fatigue Property of Titanium Alloys,” Report TDES919L - Rev. 1 by Sumitomo Metal Industries, Ltd., Japan (author unknown).
1.
Titanium Technologies, Inc, 1991, “Titanium High-Pressure Drilling Riser,” Titanium Technologies Engineering Report No. 22-012-17-9-1, Houston (author unknown);
2.
reference data in Fig. 9.3-3 by L. R. Hall, Boeing Co., and data in Fig. 9.3-8 by J. G. Bjeletich, Lockheed Missiles and Space System.
1.
Toyama
,
K.
, and
Maeda
,
T.
,
1986
, “
The Effect of Heat Treatment on the Strength and Fracture Toughness of Ti-3Al-10V-2Fe
,”
Trans. Iron Steel Inst. Jpn.
, Vol.
26
, pp.
814
821
.
2.
Turner, D. E., 1989, “Fatigue and Fracture Toughness Properties as a Function of Section Thickness for Beta Annealed Ti-6Al-4V, Eli,” Proc., 34th International SAMPE Symposium, May 8–11, pp. 290–299.
3.
Wei, R. P., Shih, T. T., and FitzGerald, J. H., 1973, “Load Interaction Effects on Fatigue Crack Growth in Ti-6Al-4V Alloy,” Nasa Contractor Report No. NASA CR-2239.
4.
Yoder
,
G. R.
,
Cooley
,
L. A.
, and
Crooker
,
T. W.
,
1978
, “
Fatigue Crack Propagation Resistance of Beta-Annealed Ti-6Al-4V Alloys of Differing Interstitial Oxygen Contents
,”
Metall. Trans. A
,
9A
, pp.
1413
1420
.
You do not currently have access to this content.